Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L4857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Dry Blend E7009 Polyvinyl Chloride, Rigid (PVC, Rigid) Recommended for whites and light pastel colors only. Not to be used for darker colors.Physical properties based on Geon E7009 white 1024 lot# UTCX 57572Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP J1000 PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000 is a compound based on Polyethersulfone resin. |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP J1000R PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000R is a compound based on Polyethersulfone resin. Added features include : Mold Release |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
32.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C @Temperature -30.0 - 100 °C |
32.8 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili.. |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
32.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
32.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | ISO 11359-1/-2 |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |