Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 65.0 - 100 µm/m-°C
36.1 - 55.6 µin/in-°F
ASTM D696
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact
Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
CTE, linear, Parallel to Flow 70.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3L PA6 (Dry)
Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing.
CTE, linear, Parallel to Flow 70.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® A4H PA66 (Dry)
Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr..
CTE, linear, Parallel to Flow 70.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3K BK00464 PA6 (Dry)
Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by..
CTE, linear, Parallel to Flow 70.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3K PA6 (Dry)
Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6.
CTE, linear, Parallel to Flow 70.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® B3L BK00464 PA6 (Dry)
Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall ..
CTE, linear, Parallel to Flow 60.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® C3U PA66/6 (Dry)
Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance.
CTE, linear, Parallel to Flow 70.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3S BK00464 PA6 (Dry)
Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
CTE, linear, Parallel to Flow 70.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® B3S HP PA6 (Dry)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing