Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 51.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 51.0 µm/m-°C
28.3 µin/in-°F
ASTM D696
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose
Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
CTE, linear, Parallel to Flow 51.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP UX06002 PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UX06002 is a compound based on Polyphthalamide resin containing Aramide Fiber, PTFE. Added features include: Easy Molding, Internally Lubricated, Heat Stabilized.
CTE, linear, Parallel to Flow 51.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
28.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT
LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant.
CTE, linear, Parallel to Flow 51.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
28.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON DX05301C PC
LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic..
CTE, linear, Parallel to Flow 51.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
28.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT
LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage.
CTE, linear, Parallel to Flow 51.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp MFK42AS PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MFK42AS is a compound based on PP resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 51.0 µm/m-°C

@Temperature 55.0 - 160 °C
28.3 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass/Mineral Reinforced PPA High Performance Polyamide Zytel HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is..
CTE, linear, Parallel to Flow 51.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starpylen MFK42AS PP, Glass/Mineral Filled, Injection Molded
Starpylen MFK42AS is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding ResinInformation provided by Eurostar.
Copyright © lookpolymers.com All Rights Reserved