Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 500 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® S600F40 NC010 PBT  (Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® SK612SF NC010 PBT  (Unverified Data**)
Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® SK615SF NC010 PBT  (Unverified Data**)
Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET  (Unverified Data**)
Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® 940 NC010 PET  (Unverified Data**)
Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66  (Unverified Data**)
Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66  (Unverified Data**)
Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6  (Unverified Data**)
Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided ..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon
Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® FG570 NC000 Acetal Homopolymer
Delrin® FG570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber for injection molding. It has high stiffness and low warpage. It has been developed for consideration in appl..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66  (Unverified Data**)
Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66  (Unverified Data**)
Zytel® FG408L NC010 is a general purpose, lubricated, impact modified polyamide 66 resin with superior toughness for injection molding applications. It has been developed for consideration into app..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6  (Unverified Data**)
Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont..
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66  (Unverified Data**)
Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 500 µm/m-°C

@Temperature 23.0 - 55.0 °C
278 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612  (Unverified Data**)
Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor..