Polymer Property : CTE, linear, Parallel to Flow = 5.50 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 5.50 µm/m-°C

@Temperature 23.0 - 80.0 °C
3.06 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® S 4090 G2 10% Glass Filled PBT
Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers..