Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 84.0 µm/m-°C | 46.7 µin/in-°F | ASTM D696 |
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
CTE, linear, Parallel to Flow | 84.0 µm/m-°C | 46.7 µin/in-°F | ASTM D696 |
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol.. |
|||
CTE, linear, Parallel to Flow | 84.0 µm/m-°C @Temperature 20.0 °C |
46.7 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 105-28 Cellulose Acetate
(discontinued **) 28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Parallel to Flow | 84.0 µm/m-°C @Temperature 20.0 °C |
46.7 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 132E-28 Cellulose Acetate
(discontinued **) 28% Plasticized with 25% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Parallel to Flow | 84.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
46.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 84.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
46.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 84.0 µm/m-°C @Temperature 20.0 °C |
46.7 µin/in-°F @Temperature 68.0 °F |
ISO data |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |