Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 46.0 µm/m-°C | 25.6 µin/in-°F | ASTM D696 |
PolyOne Nanoblend™ LST 5571 Polypropylene, Unspecified (PP, Unspecified) Nanoblend compounds, formerly known as Maxxam LST, are LIGHT, STIFF AND TOUGH. Using nanoclay technology, these compounds deliver a combination of high stiffness and impact resistance to meet demand.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Extem UH1016M TPI Blend High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.6 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C | 25.6 µin/in-°F | ASTM D696 |
PolyOne Geon™ L6105 natural Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
25.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C | 25.6 µin/in-°F | ASTM D696 |
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing milled Glass and PTFE. Added features include; Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C | 25.6 µin/in-°F | ISO 11359 |
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry) Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low.. |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C | 25.6 µin/in-°F | ISO 11359 |
BASF Ultramid® 8260 HS PA6 (Dry) |
|||
CTE, linear, Parallel to Flow | 46.0 µm/m-°C @Temperature 20.0 °C |
25.6 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi.. |