Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature -30.0 - 120 °C
36.7 µin/in-°F

@Temperature -22.0 - 248 °F
ISO 11359
Nyco NYGLOS® 4W STO105 Wollastonite in Polypropylene
Data for polypropylene reinforced with 15% Nyco NYGLOS® 4W STO105 Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3)..
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX1814N PC
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® LUX1832 PC
MFR=3.0; Branched extrusion grade for LED applications, UV stabilized; available in diffuse colors
CTE, linear, Parallel to Flow 66.0 µm/m-°C
36.7 µin/in-°F
ASTM D696
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy)
Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
36.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Faradex AS0029 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS-1002 FR is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: Flame Retardant, EM..
CTE, linear, Parallel to Flow 66.0 µm/m-°C
36.7 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ N1002A-M41 Nylon
Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11
LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity.
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature -30.0 - 100 °C
36.7 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP
SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold..
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11
LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity.
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MF006AS PP
LNP THERMOCOMP* MF006AS is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Parallel to Flow 66.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP
LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.