Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 520 µm/m-°C @Temperature 23.0 - 60.0 °C |
289 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |