Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL920 PC Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
15.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL920 PC (Asia Pacific) Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V25 NAT BA PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: Asia PacificProduct Application.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® TPX-HTN-01031 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 35% Filler by WeightAdditive: Heat Stabilizer Features: Flame Retardant, Heat Stabilized and High Temperature Strength UL .. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PES GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP E GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled, Heat Stabilized and High Viscosit.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA4/6 CF30 TL15 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance and Low FrictionInformation p.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 GF15 TL15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilized and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 GF40 ML2 HS UV BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized, Molybdenum Disulfide Lubricant and UV StabilizerFeatures: Lubricated, Good .. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 GF40 ML5 HS 12 mm 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerAp.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced. Flame retardant. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced, flame retardant material. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 20.0 °C |
15.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Sumitomo Bakelite North America RX® 431 Cellulose Reinforced Phenolic Novolac RX431 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RF008U PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF008U is a compound based on PA 66 resin containing Glass Fiber. Added features include; UV-Stabilized, Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG6ST01 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG6ST01 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
15.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG6ST01 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG6ST01 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 27.0 µm/m-°C | 15.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PPA CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low.. |