Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 2.20 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.22 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
CTE, linear, Parallel to Flow 2.20 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.22 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
CTE, linear, Parallel to Flow 2.20 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.22 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
CTE, linear, Parallel to Flow 2.20 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.22 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
CTE, linear, Parallel to Flow 2.20 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.22 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:..
CTE, linear, Parallel to Flow 2.20 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.22 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
CTE, linear, Parallel to Flow 2.20 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.22 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
CTE, linear, Parallel to Flow 2.20 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
1.22 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..