Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
LyondellBasell Lupolen® 4261 A HDPE, Blow Molding Grade
Easy-to-process bow molding grade for technical containers such as fuel tanks, petrol filler inlets, expansion tanks, horticultural spray tanks, tanks for lawnmowers, disposable containers (up to 10..
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 23.0 - 55.0 °C
94.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Covestro Desmopan® 356 Thermoplastic Polyurethane
Desmopan 356 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer Mat..
CTE, linear, Parallel to Flow 170 µm/m-°C
94.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4158 nat PA612
Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo..
CTE, linear, Parallel to Flow 170 µm/m-°C
94.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4180 black 9992 PA1010
Product description: Grilamid XE 4180 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 black 9992 is highly ..
CTE, linear, Parallel to Flow 170 µm/m-°C
94.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4180 nat PA1010
Product description: Grilamid XE 4180 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 NATURAL is highly resist..
CTE, linear, Parallel to Flow 170 µm/m-°C
94.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4181 black PA1010
Product description: Grilamid XE 4181 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 black 9992 is highly ..
CTE, linear, Parallel to Flow 170 µm/m-°C
94.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4181 nat PA1010
Product description: Grilamid XE 4181 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 natural is highly resist..
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 55.0 - 160 °C
94.4 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® LT 6040IH Nylon (Conditioned)
ISO data provided by the manufacturer, Arkema.
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® LT 6040ISH Nylon (Conditioned)
ISO data provided by the manufacturer, Arkema.
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Arkema Group Pebax® 5533 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE(PEBA) hardness 55 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: overmolded parts for sport good (Footba..
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Covestro Texin® 255 Urethane Thermoplastic Elastomer
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop..
CTE, linear, Parallel to Flow 170 µm/m-°C

@Temperature 20.0 °C
94.4 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® LT 6040 Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good ..