Polymer Property : CTE, linear, Parallel to Flow = 111 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer
Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer
Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer
Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer
Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
ASTM D696
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, ..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
ASTM D696
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
ASTM D696
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
ASTM D696
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)  (Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..