Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 106 µm/m-°C @Temperature 20.0 °C |
58.9 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 105-33 Cellulose Acetate
(discontinued **) 33% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Parallel to Flow | 106 µm/m-°C @Temperature 23.0 - 100 °C |
58.9 µin/in-°F @Temperature 73.4 - 212 °F |
|
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear, Parallel to Flow | 106 µm/m-°C @Temperature 20.0 °C |
58.9 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, Dry as Molded Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
CTE, linear, Parallel to Flow | 106 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR6300 AES+PC+SAN (Asia Pacific) Wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
CTE, linear, Parallel to Flow | 106 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY Lexan_WR6300 AES+PC+SAN LNP* Lubriloy* Lexan_WR6300 compound is a wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
CTE, linear, Parallel to Flow | 106 µm/m-°C @Temperature -30.0 - 30.0 °C |
58.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked. |
|||
CTE, linear, Parallel to Flow | 106 µm/m-°C @Temperature 23.0 - 60.0 °C |
58.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp M10009A PP (Europe-Africa-Middle East) LNP* STARFLAM* M10009A is a compound based on Polypropylene resin, containing Flame Retardant. Added features include : Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
CTE, linear, Parallel to Flow | 106 µm/m-°C @Temperature 23.0 - 60.0 °C |
58.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |