Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX39F ABS
Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EXABS01 ABS
Sheet extrusion ABS with medium impact.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® GX3800F ABS
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58 ABS
High impact ABS for sheet extrusion and blow molding applications.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58F ABS
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific)
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature 20.0 °C
56.1 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Centrex® 833 ASA+AES Blend  (discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi..
CTE, linear, Parallel to Flow 101 µm/m-°C
56.0 µin/in-°F
ASTM D696
Techmer ES HiFill FR® PBT/ABS FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -30.0 - 30.0 °C
56.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP HX03408 PA11
LNP* Thermocomp* HX03408 is a compound based on Nylon 11 containing Proprietary Fillers. Added feature includes: Clean Compound System
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® EX39 ABS
Highest impact extrusion ABS for sheet and blow molding applications.
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature 20.0 °C
56.1 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 105-23 Cellulose Acetate  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical