Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
10.6 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 20.0 °C |
10.6 µin/in-°F @Temperature 68.0 °F |
ASTM E381 |
Solvay Specialty Polymers Kadel® E-1130 Polyketone
(discontinued **) High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
10.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V9561 PET Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
10.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific) DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF006A PPS (Europe-Africa-Middle East) LNP* Thermocomp* OF-1006 is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
10.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF009AXP PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF009AXP is a compound based on Polyphthalamide resin containing 45% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 20.0 °C |
10.6 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America E 3938A Hardware Grade Epoxy Fiberglass reinforced epoxy molding compound with excellent dimensional stability, good strength and excellent electrical insulation properties.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 20.0 °C |
10.6 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America RX® 3-1-525F-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
10.6 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Thickness 1.50 mm, Temperature 55.0 - 160 °C |
10.6 µin/in-°F @Thickness 0.0591 in, Temperature 131 - 320 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C | 10.6 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
10.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C | 10.6 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C | 10.6 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530L NC010 Polyethylene Terephthalate (PET) Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
10.6 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
10.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon PX98038 PA 6 (Europe-Africa-Middle East) LNP* STATKON* PX98038 is a compound based on PA6 resin containing Carbon Fiber, Glass Fiber, Flame Retardant. Added features include : Flame Retardant, Electrically Conductive, Heat Stabilized.This .. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
10.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 20.0 °C |
10.6 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat.. |
|||
CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature 20.0 °C |
10.6 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 6030 Nylon 6 Alloy, 30% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |