Polymer Property : CTE, linear, Parallel to Flow = 0.504 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 0.504 µm/m-°C

@Temperature -30.0 - 100 °C
0.280 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM E831
ExxonMobil Exxtral™ BMV 201 Performance Polyolefin
Product Description: A specialty thermoplastic olefin injection molding compound resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for large automotive e..
CTE, linear, Parallel to Flow 0.504 µm/m-°C

@Temperature -30.0 - 100 °C
0.280 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM E831
ExxonMobil Exxtral™ H1725 Performance Polyolefin
Product Description: A specialty thermoplastic olefin compound resin with good flow, cold temperature resistance, high flexural modulus, low CLTE, and excellent paintability for automotive exterior ..