Polymer Property : Heat of Fusion = 59.0 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 59.0 J/g
25.4 BTU/lb
ASTM E793
Eastman CB12 PET  (discontinued **)
Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov..
Heat of Fusion 59.0 J/g
25.4 BTU/lb
Crystallization Heat
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound  (discontinued **)
Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall..
Heat of Fusion 59.0 J/g
25.4 BTU/lb
Crystallization Heat
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound  (discontinued **)
Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
Heat of Fusion 59.0 J/g
25.4 BTU/lb
Crystallization Heat
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound  (discontinued **)
Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate..
Heat of Fusion 59.0 J/g
25.4 BTU/lb
DSC on the first heating cycle; ASTM E793
DAK Americas Laser+® MB912 PET
Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient pr..
Heat of Fusion 59.0 J/g
25.4 BTU/lb
Crystallization Heat
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer  (discontinued **)
Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
Heat of Fusion 59.0 J/g
25.4 BTU/lb
ASTM E793
Eastman VersaTray 12822 Plastic  (discontinued **)
VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo..