Polymer Property : Heat of Fusion = 37.0 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 37.0 J/g
15.9 BTU/lb
80°C to end of melting
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
Heat of Fusion 37.0 J/g
15.9 BTU/lb
Crystallization Heat
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer  (discontinued **)
Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD..