Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 18.0 - 26.0 J/g | 7.74 - 11.2 BTU/lb | Crystallization Heat; DSC |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Heat of Fusion | 18.0 - 26.0 J/g | 7.74 - 11.2 BTU/lb | DSC |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Heat of Fusion | 18.0 - 26.0 J/g | 7.74 - 11.2 BTU/lb | Crystallization Heat; DSC |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Heat of Fusion | 18.0 - 26.0 J/g | 7.74 - 11.2 BTU/lb | DSC |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |