Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 66.0 - 79.0 °C | 151 - 174 °F | Dip |
ChevronTexaco Compound H Rust Proof Texaco Rust Proof Compounds deliver value through:Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the.. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12028 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12032 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12038 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12050 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12062 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12026 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12034 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12036 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12046 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Minimum Service Temperature, Air | 66.0 °C | 151 °F | Long term |
3M 12030 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |