Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 4.40 °C | 39.9 °F | |
3M Controltac™ 160 Graphic Film 4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha.. |
|||
Minimum Service Temperature, Air | 4.40 °C | 39.9 °F | |
3M Controltac™ 8640C ES Graphic Film with Comply™ Adhesive This 4-mil film offers great versatility along with slidable, repositionable, pressure activated adhesive. This long term durable and removable film has excellent hiding power and stability, making .. |
|||
Minimum Service Temperature, Air | 4.40 °C | 39.9 °F | |
3M Controltac™ IJ160C Graphic Film with Comply™ Adhesive 4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels .. |
|||
Minimum Service Temperature, Air | 4.40 °C | 39.9 °F | |
3M Scotchcal™ 3470 Graphic Film 4-mil, opaque white and opaque black, vinyl film with a matte finish; Pressure-sensitive adhesive; Excellent hiding power; Removable with heatInformation provided by 3M |
|||
Minimum Service Temperature, Air | 4.40 °C | 39.9 °F | |
3M Controltac™ 160C Graphic Film with Comply™ Adhesive 4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha.. |
|||
Minimum Service Temperature, Air | 4.40 °C | 39.9 °F | |
3M Controltac™ IJ160 Graphic Film 4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels .. |
|||
Minimum Service Temperature, Air | 4.40 °C | 39.9 °F | |
3M Scotchcal™ 3475 Graphic Film 4-mil, opaque white and opaque black, vinyl film with a matte finish; Pressure-sensitive adhesive; Excellent hiding power; Removable with heatInformation provided by 3M |