Polymer Property : Minimum Service Temperature, Air = 22.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -5.10 °C
22.8 °F
Gehman torsion test, T10
Daikin DAI-EL G-912 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content
Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good compression set.Information provided by Daikin Industries.