Thermal Properties Metric English Comments
Minimum Service Temperature, Air -5.50 °C
22.1 °F
3M Panagraphics™ III Wide Width Flexible Substrate
22 mil white-pigmented vinyl substrate with a polyester scrim; Smooth front surface with a semi-gloss finish; Decorate first or second surface with inkjet direct printing or first surface with cut f..