Thermal Properties Metric English Comments
Minimum Service Temperature, Air 66.0 - 79.0 °C
151 - 174 °F
Dip
ChevronTexaco Compound H Rust Proof
Texaco Rust Proof Compounds deliver value through:Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12028 Black 1/8" (3.2 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12032 Black 3/32" (2.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12038 Black 3/8" (9.5 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12049 Black 3/8" (9.5 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12050 Black 1/2" (12.7 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12062 Black 3/32" (2.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12026 Black 1/16" (1.6 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12034 Black 1/4" (6.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12036 Black 3/16" (4.8 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12046 Black 1/16" (1.6 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12048 Black 1/8" (3.2 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12054 Black 1/4" (6.4 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
3M 12030 Black 1/2" (12.7 mm) Polyurethane Foam
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance ..