Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | Recommended |
Nye Lubricants 708C (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | Recommended |
Nye Lubricants 710R Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | Recommended |
Nye Lubricants NYOSIL-M25 Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | Recommended |
Nye Lubricants NYOSIL-M25UV Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | |
Dow Corning MOLYKOTE® 33 EXTREME LOW TEMPERATURE BEARING GREASE, LIGHT Phenyl-methyl silicone grease for extreme low temperaturesInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | |
Aremco Pyro-Tape™ 682-HR High Temperature Tape Bi-layer aluminum/fiberglass with silicone adhesive Applications Heat Reflection Features Protective wrap for pipes exposed to high heat. Heat mask for process instrumentation. Protective wrap for chutes, rails and slides. |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | |
3M 5151 PTFE Glass Cloth Tape 3M™ PTFE Glass Cloth Tape 5151 is constructed using (PTFE) polytetra-fluoroethylene impregnated glass cloth and silicone adhesive. This tape is used in many applications requiring high temperature .. |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | |
3M 5451 PTFE Glass Cloth Tape 3M™ PTFE Glass Cloth Tape 5451 has a silicone adhesive which provides a high temperature release surface for protection and insulation.Information provided by 3M |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | |
3M 5453 PTFE Glass Cloth Tape 3M™ PTFE Glass Cloth Tape 5453 has a silicone adhesive which provides a high temperature release surface for protection and insulation.Information provided by 3M |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | |
Aremco Pyro-Tape™ 682-PM High Temperature Tape Tri-layer silicone rubber/aluminum foil/ fiberglass with silicone adhesive Applications Plasma Spray Masking Features Multi-ply construction replaces single-ply tapes permitting significant reduction in masking time. Shadow mask tape for HVOF (high velocity oxy- fuel) spr.. |
|||
Minimum Service Temperature, Air | -73.0 °C | -99.4 °F | |
3M 5153 PTFE Glass Cloth Tape 3M™ PTFE Glass Cloth Tape 5151 is constructed using (PTFE) polytetra-fluoroethylene impregnated glass cloth and silicone adhesive. This tape is used in many applications requiring high temperature .. |