Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -38.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -38.0 °C
-36.4 °F
P & P Technology KE Series Cored Shielding Mesh Gasket Strip
Cover: Knitted Monel To BS 3075-NA 13 0.11mm Dia 2 Layers. Core Material: Neoprene closed cell sponge.Information provided by P & P Technology
Minimum Service Temperature, Air -38.0 °C
-36.4 °F
JIS-K-6723
Denka REOMER G G3010 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Minimum Service Temperature, Air -38.0 °C
-36.4 °F
JIS-K-6723
Denka VINYKON S210070 PVC, S grade for transparent extrusion molding
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Minimum Service Temperature, Air -38.0 °C
-36.4 °F
JIS-K-6723
Denka LCS Z6060 Thermoplastic Elastomer, Injection Molding Grade (general)
"DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r..
Copyright © lookpolymers.com All Rights Reserved