Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | |
Process Technologies Inc Viton® Extreme™ Compound 2001 Sanitary Gasket/O-Ring Process Technologies Viton® Extreme sanitary gaskets and O-Rings are produced from formulated Viton® Extreme ETP-600S fluoroelastomer. This unique material is produced with Advanced Polymer Archi.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | JIS-K-6723 |
Denka REOMER G G8250 Thermoplastic Elastomer, For Injection Molding Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | JIS-K-6723 |
Denka VINYKON S210085 PVC, S grade for transparent extrusion molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | JIS-K-6723 |
Denka VINYKON W1022 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | JIS-K-6723 |
Denka VINYKON W1051 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | JIS-K-6723 |
Denka VINYKON W1080 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | JIS-K-6723 |
Denka VINYKON W5230 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | Service |
3M 7710 Acetate Identification Label Material 3M™ Label Material 7710 gloss clear acetate with 3M™ 400 high tack acrylic adhesive offers consistent, high quality appearance and excellent UV resistance. The transparent film easily die-cuts whi.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | JIS-K-6723 |
Denka VINYKON S210050 PVC, S grade for transparent extrusion molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | |
ChevronTexaco Ulti-Plex® NLGI 0 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | |
ChevronTexaco Ulti-Plex® NLGI 1 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |
|||
Minimum Service Temperature, Air | -26.0 °C | -14.8 °F | |
ChevronTexaco Ulti-Plex® NLGI 2 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |