Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | Torsion Stiffness Temperature |
Stir SpA Giesse EPM/75 (PVC) Application: Extrusion medical parts - medium/high flexibilityInformation provided by STIR SpA |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | Gehman T100 |
Zeon Chemicals HyTemp® AR72LF AR Polyacrylate Elastomer HyTemp AR72LF contains acrylic esters with a small percentage of chlorine cure site monomer. Vulcanizates have excellent oil, heat, and compression set resistance with good low temperature.Excellent.. |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | JIS-K-6723 |
Denka REOMER G G3012 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | JIS-K-6723 |
Denka VINYKON M557050 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | JIS-K-6723 |
Denka VINYKON W4800 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | JIS-K-6723 |
Denka VINYKON W7300E PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | Service |
3M CP 25WB+ Fire Barrier Sealant 3M Fire Barrier Sealant CP 25WB+ is a high-performance, ready-to-use, gun-grade, latex-based, intumescent sealant that dries to form a monolithic fire-stop seal that also acts as a barrier to airbor.. |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | Service |
3M IC 15WB+ Fire Barrier Sealant 3M Fire Barrier Sealant IC 15WB+ is a cost-effective, one-part, gun-grade, latex-based, intumescent firestop sealant that dries to form a monolithic firestop seal that also acts as a barrier to airb.. |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | Service |
3M FD 150+ Fire Barrier Sealant 3M Fire Barrier Sealant FD 150+ is an economical, ready to use, gun-grade, elastomeric sealant that dries to from a monolithic flexible firestop seal. 3M Fire Barrier Sealant FD 150+ firestops joint.. |
|||
Minimum Service Temperature, Air | -28.0 °C | -18.4 °F | JIS-K-6723 |
Denka VINYKON M556050 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |