Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -115 - -40.0 °C | -175 - -40.0 °F | Average value: -68.5 °C Grade Count:32 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |
|||
Minimum Service Temperature, Air | -115 °C | -175 °F | Continuous useful temperature. |
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -115 °C | -175 °F | Continuous useful temperature. |
Momentive Performance Materials RTV511 White Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -115 °C | -175 °F | Continuous useful temperature. |
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -115 °C | -175 °F | Continuous useful temperature. |
Momentive Performance Materials RTV566 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -115 °C | -175 °F | Continuous useful temperature. |
Momentive Performance Materials RTV567 Translucent Extreme Low Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Minimum Service Temperature, Air | -115 °C | -175 °F | Continuous useful temperature. |
Momentive Performance Materials RTV6156 Clear Potting/Encapsulating Gel Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Minimum Service Temperature, Air | -115 °C | -175 °F | Continuous useful temperature. |
Momentive Performance Materials RTV656 Clear Extreme Low Temperature Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Minimum Service Temperature, Air | -115 °C | -175 °F | |
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material.. |