Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 104 °C | 219 °F | ExxonMobil Method |
ExxonMobil LL 1002.32 Cast Film Resin
(discontinued **) LL 1002.32 is a butene LLDPE resin designed for the cast film process. Films made from LL 1002.32 have very good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Crystallization Temperature | 104 °C | 219 °F | ASTM D1525 |
LG Chemical LUTENE FB0300 LDPE Blown Film Grade Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e.. |
|||
Crystallization Temperature | 104 °C | 219 °F | ASTM D1525 |
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific.. |
|||
Crystallization Temperature | 104 - 115 °C | 219 - 239 °F | Average value: 110 °C Grade Count:7 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |