Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 93.0 - 97.0 °C | 199 - 207 °F | |
Addcomp PRIEX® Ionomer 48101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Crystallization Temperature | 93.0 - 97.0 °C | 199 - 207 °F | |
Addcomp PRIEX® Ionomer 45101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |