Polymer Property : Crystallization Temperature = 203 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 95.0 °C
203 °F
ExxonMobil Method
ExxonMobil LD 103.MP Industrial Film Resin  (discontinued **)
LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati..
Crystallization Temperature 95.0 °C
203 °F
ExxonMobil Method
ExxonMobil LD 146.NH Cast Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Crystallization Temperature 95.0 °C
203 °F
ExxonMobil Method
ExxonMobil LD 146.NH Packaging Film Resin  (discontinued **)
LD 146.NH is a homopolymer film resin offering good clarity, toughness, and stiffness. It is used in food packaging and laminating film.Information provided by ExxonMobil Chemical
Crystallization Temperature 95.0 °C
203 °F
Dow Method (DSC)
Dow 722 Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c..
Crystallization Temperature 95.0 - 104 °C
203 - 219 °F
Average value: 98.4 °C Grade Count:10
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..
Copyright © lookpolymers.com All Rights Reserved