Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 91.0 °C | 196 °F | ExxonMobil Method |
ExxonMobil LD 312.09 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Crystallization Temperature | 91.0 °C | 196 °F | ExxonMobil Method |
ExxonMobil LD 312.23 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Crystallization Temperature | 91.0 °C | 196 °F | ExxonMobil Method |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
Crystallization Temperature | 91.0 °C | 196 °F | ExxonMobil Method |
ExxonMobil LD 334.57 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Crystallization Temperature | 91.0 °C | 196 °F | ExxonMobil Method |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |