Crystallization Temperature 132 °C
270 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Crystallization Temperature 132 °C
270 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF)
Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 ..