Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D-1525 |
Plaskolite Optix® CA - 51 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D-1525 |
Plaskolite Optix® CA - 51 HF OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D-1525 |
Plaskolite Optix® CA - 51 HF UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 51 HF OG General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 51 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 51 HF UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D1525 |
LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade ApplicationsMicrothene MP564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. MP564189 is 16 mesh powder.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D1525 |
I. Stern N2560 General Purpose Crystal Polystyrene Features:Excellent ClarityExcellent Process PropertiesHigh Heat MoldingApplicationsMedical PartsDomestic AppliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRF 3705 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Medium Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D1525 |
ExxonMobil EXXCO™ Exxco 012 w/20% LDPE Enhanced Performance Extrusion Coating Resin Exxco 012 PE resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. It offers outstanding adhesion to many substrates, along with excellent hot tack and heat seal stre.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D1525 |
ExxonMobil LD 506.07 Compounding and molding resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D1525 |
ExxonMobil LDPE LD 506.07 Low Density Polyethylene Resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ISO 306 |
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade) Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock.. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ISO 306 |
ExxonMobil LDPE LD 653 Low Density Polyethylene Resin (European Grade) Product Description: LD 653 is an easy flowing LDPE grade with medium stiffness and good toughness.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: .. |
|||
Vicat Softening Point | 91.1 °C | 196 °F | 50°C/hr; 10N; ASTM D1525 |
Arkema Group Solarkote® H300 Acrylic Superior UV protection, Adhesion to HIPS, ASTM Classification PMMA 0233V3Information provided by Arkema Group |
|||
Vicat Softening Point | 91.1 °C | 196 °F | ASTM D1525 |
ExxonMobil EXXCO™ Exxco 012 w/40% LDPE Enhanced Performance Extrusion Coating Resin Exxco 012 PE resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. It offers outstanding adhesion to many substrates, along with excellent hot tack and heat seal stre.. |