Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 77.0 - 86.0 °C | 171 - 187 °F | Average value: 81.9 °C Grade Count:11 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Vicat Softening Point | 84.0 - 86.0 °C @Load 5.00 kg |
183 - 187 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 321 Rigid PVC, Antishock Extrusion Lead Free Outdoor antishock profiles |
|||
Vicat Softening Point | 68.0 - 86.0 °C | 154 - 187 °F | Average value: 77.5 °C Grade Count:26 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |