Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 73.9 °C | 165 °F | ASTM D1525 |
ExxonMobil Escor™ 5070 Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5070 is an ethylene acrylic acid copolymer characterized by high melt index and 9% acrylic acid comonomer content. Escor 5070 combines easily processing and adhesion to po.. |