Thermal Properties Metric English Comments
Vicat Softening Point 55.0 °C

@Load 1.00 kg
131 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene
Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:..
Vicat Softening Point 55.0 °C
131 °F
ISO 306/B50
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
Vicat Softening Point 55.0 °C
131 °F
Vicat A, 1 kg; DIN 53460/ISO 306
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber  (discontinued **)
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Westlake EMAC® SP2405 20% Ethylene-Methyl Acrylate Copolymer  (discontinued **)
Westlake EMAC® SP2405 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperature are required. SP2405 provides..
Vicat Softening Point 55.0 °C
131 °F
1000g; ASTM D-1525
ExxonMobil Escorene® LD-723 High EVA Extrusion Coating Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Huntsman IROGRAN® PS455-203 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Vicat Softening Point 55.0 °C
131 °F
(A50 (50°C/h 10 N)); ISO 306
LyondellBasell Adflexâ„¢ Q 100 F Polyolefin
Description: Adflexâ„¢ Q 100 F is a thermoplastic polyolefin which has been developed for the extrusion of blown film, it is also suitable for sheet extrusion. Adflexâ„¢ Q 100 F features a ver..
Vicat Softening Point 55.0 °C

@Load 5.00 kg
131 °F

@Load 11.0 lb
LATI Latigea B01 I8 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...
Vicat Softening Point 55.0 °C
131 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Westlake EBAC® Plus SP1903 18% Ethylene Butyl Acrylate Copolymer
Westlake EBAC® SP1903 is an 18% EBA copolymer designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1903 provides excel..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer
Description: Westlake EBAC® SP1806 is an ethylene butyl acrylate copolymer designed for extrusion coating and laminating. SP1806 can also be compounded as an impact modifier or used in highly fill..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Westlake EMAC® SP2205 20% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2205 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2205 provide..
Vicat Softening Point 55.0 °C
131 °F
ASTM D-1525
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane
Features: Hard, flexible, abrasion resistant coatings. Primarily used for all solution binder for inks and lacquers on fabrics and various substrates.Uses: Adhesives and inks & lacquers, pigment bin..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excelle..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
ExxonMobil EXACT™ 4049 Plastomer for Elastic Film and Elastic Film Blends
Product Description: Exact 4049 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed for use as the cling component in mul..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525, ISO 306
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate
Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a ..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525, ISO 306
DuPont™ Elvax® 3155 Ethylene Vinyl Acetate
DuPont™ Elvax® 3155 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 31..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
Arkema Group Orevac® 9304 Film EVA-MAH Terpolymer
EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group
Vicat Softening Point 55.0 °C
131 °F
BASF Procom® D 1146 Polypropylene
Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 55.0 °C
131 °F
BASF Procom® D 1158 Polypropylene
Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 55.0 °C
131 °F
BASF Procom® D 1165 Polypropylene
Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process ..
Vicat Softening Point 55.0 °C
131 °F
Rate B; ASTM D-1525
ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.Excellent abrasion resistance, impact strength, hardness, and tensile strength. Iotek ionomers provide superb low temperature impact strength when ..
Vicat Softening Point 55.0 °C
131 °F
ASTM D1525
DuPont Bynel® 2169 Anhydride-Modified Ethylene Acrylate Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
Vicat Softening Point 55.0 - 160 °C
131 - 320 °F
Average value: 111 °C Grade Count:6
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..
Vicat Softening Point 55.0 °C

@Load 5.00 kg
131 °F

@Load 11.0 lb
LATI Latigea B01 I6 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p...
Copyright © lookpolymers.com All Rights Reserved