Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 47.1 °C | 117 °F | ASTM D1525 |
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Vicat Softening Point | 47.1 °C | 117 °F | ASTM D1525 |
ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film Product Description: Vistamaxx 6202FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution, and is produced us.. |
|||
Vicat Softening Point | 47.1 - 167 °C | 117 - 333 °F | Average value: 72.2 °C Grade Count:8 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |