Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 216 °C | 421 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilitop BT G4 FR C3 is a 20% Glass Fiber Reinforced, Flame Retardant PBT Description: Nilitop BT G4 FR C3 is a 20% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It.. |
|||
Vicat Softening Point | 216 °C | 421 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2312EPR PEI 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Vicat Softening Point | 216 °C | 421 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Vicat Softening Point | 216 °C | 421 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® GP-5300G PBT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 126F6 Nylon 6, 30% Glass Fiber SAXAMID 126F6 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Other properties are .. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri.. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 126F7 Nylon 6, 35% Glass Fiber SAXAMID 126F7 is a polyamide 6 injection-molding-grade reinforced with 35% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Additional properties.. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 126F8 Nylon 6, 40% Glass Fiber SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers |
|||
Vicat Softening Point | 216 °C | 421 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 126F10 Nylon 6, 50% Glass Fiber SAXAMID 126F10 is a polyamide 6 injection-molding-grade reinforced with 50% glass fibers.Information provided by SAX Polymers |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 126F9 Nylon 6, 45% Glass Fiber SAXAMID 126F9 is a polyamide 6 injection-molding-grade reinforced with 45% glass fibers.Information provided by SAX Polymers |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 216 °C | 421 °F | B/120; ISO 306 |
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 216 °C | 421 °F | ASTM D1525 |
Ashley Polymers Ashlene® 279 PPO Alloy A general purpose, paintable injection molding grade with high chemical resistance and mechanical performance. Good heat resistance with dimensional stability in dark gray or black only.Data provid.. |