Thermal Properties Metric English Comments
Vicat Softening Point 208 °C
406 °F
B
Plastcom SLOVAMID 66/6 T 30 TS PA66/6, 30% mineral filling
FeaturesPA 66/PA 6 alloy with the content of 30 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, autom..
Vicat Softening Point 208 °C
406 °F
9.8 N; ISO 306, ASTM D1525
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
Vicat Softening Point 208 °C
406 °F
Rate B/120; ISO 306
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound
Vicat Softening Point 208 °C
406 °F
Rate B/50; ISO 306
SABIC Innovative Plastics ULTEM 4001 PEI (Europe-Africa-Middle East)
PTFE filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
Vicat Softening Point 208 °C
406 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Ultem ATX202R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 208 °C
406 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 208 °C
406 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Vicat Softening Point 208 °C
406 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 4012G PBT
VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
Vicat Softening Point 208 °C
406 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East)
VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009. 30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 208 °C
406 °F
Rate B/50; ISO 306
SABIC Innovative Plastics LNP THERMOCOMP PF004 PA 6 (Europe-Africa-Middle East)
20% glass fibre reinforced Polyamide 6 injection moulding resin.
Vicat Softening Point 208 °C
406 °F
B/50; ISO 306
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded
BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Vicat Softening Point 208 °C
406 °F
B/50; ISO 306
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded
BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.