Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 180 °C | 356 °F | ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Vicat Softening Point | 180 °C | 356 °F | B |
Plastcom SLOVAMID 6 HI/1 TLS PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Vicat Softening Point | 180 °C | 356 °F | VST/A/50; ASTM D1525 |
GEHR Plastics ECOGEHR® PA 11 Nylon 11 Conditioned
(discontinued **) Nylon 11 is made 100% from the components of castor oil, and is thus wholly bio-based. ECOGEHR® Nylon 11 possesses similar properties to Nylon 12, and an excellent status with respect to applicatio.. |
|||
Vicat Softening Point | 180 °C | 356 °F | 50°C/h 50N; ISO 306 |
Lanxess Durethan® BC 30 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, rapid processing, higher notched impact strength than B 30 S / B 31 SK in dry and conditioned state, impact-modified |
|||
Vicat Softening Point | 180 °C | 356 °F | 50°C/h 50N; ISO 306 |
Lanxess Durethan® BC 40 SR2 000000 Nylon 6 PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified |
|||
Vicat Softening Point | 180 °C | 356 °F | 50°C/h 50N; ISO 306 |
Lanxess Pocan® B 1501 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |
|||
Vicat Softening Point | 180 °C | 356 °F | 50°C/h 50N; ISO 306 |
Lanxess Pocan® B 1505 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Vicat Softening Point | 180 °C @Load 5.00 kg |
356 °F @Load 11.0 lb |
|
LATI Latamid SP1 PA 6.10 Polyamide 6.10 (PA6.10). Unfilled. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Vicat Softening Point | 180 °C @Load 5.00 kg |
356 °F @Load 11.0 lb |
|
LATI Latigray 62-01 CX/75 PA 6 Radiopaque compound based on Polyamide 6 (PA6). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem ATX100R PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | >= 180 °C | >= 356 °F | ISO 306 |
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS) Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis.. |
|||
Vicat Softening Point | >= 180 °C | >= 356 °F | ISO 306 |
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS) Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista.. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East) DATA ON BK1005 ONLY. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications.. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Asia Pacific) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Vicat Softening Point | 180 °C | 356 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V3500EX PBT PBT, Flame Retardant, Heat Stabilized, Extrusion grade for monofilament/Fiber ApplicationThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 180 °C | 356 °F | ASTM D1525 |
Toyobo PELPRENE™ P90B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Vicat Softening Point | 180 °C | 356 °F | 50°C/hr; 50N |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Vicat Softening Point | 180 °C | 356 °F | 50°C/h 50N; ISO 306 |
Lanxess Pocan® B 1600 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |