Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXM4701 PPC LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Americas .. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 4704 PC (Europe-Africa-Middle East) High heat resistant polycarbonate copolymer, provides of 165 C at 1.82 MPa. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with bi.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Vicat Softening Point | 170 - 215 °C | 338 - 419 °F | Average value: 198 °C Grade Count:23 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Average value: 170 °C Grade Count:4 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Vicat Softening Point | 170 °C | 338 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50-8025 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem ATX100R PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB Listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific) Low odor grade for IC tray application |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Vicat Softening Point | 170 °C | 338 °F | 1kg load; ASTM D1525 |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Vicat Softening Point | 170 °C | 338 °F | 1kg load; ASTM D1525 |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
Vicat Softening Point | 170 °C | 338 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6000/50 HWUVCP Nylon 6, Impact Modified Until 0°C, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 170 °C | 338 °F | 50 °C/h 50N; ISO 306 |
DSM Arnitel® CM551 TPC-ES Heat Resistant Copolyester |
|||
Vicat Softening Point | 170 °C @Load 5.00 kg |
338 °F @Load 11.0 lb |
|
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Vicat Softening Point | 170 - 205 °C | 338 - 401 °F | Average value: 186 °C Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Vicat Softening Point | 170 °C @Load 5.00 kg |
338 °F @Load 11.0 lb |
|
LATI Latimass 62-01 D025 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |