Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 135 - 159 °C | 275 - 318 °F | Average value: 150 °C Grade Count:3 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Vicat Softening Point | 78.0 - 159 °C | 172 - 318 °F | Average value: 141 °C Grade Count:18 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |