Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 23.0 - 127 °C | 73.4 - 261 °F | Average value: 64.9 °C Grade Count:66 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Vicat Softening Point | 95.0 - 127 °C | 203 - 261 °F | ASTM D1525 |
Micropol Microlink XL Crosslinkable Polyethylene Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi.. |
|||
Vicat Softening Point | 114 - 127 °C | 237 - 261 °F | Average value: 119 °C Grade Count:4 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |