Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 253 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 253 °C
487 °F
49 N; ISO 306, ASTM D1525
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66
Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
Vicat Softening Point 253 °C
487 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1/CF/10/GK/20/TF/5/BK Polyamide 66, with carbon fiber, glass spheres and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Vicat Softening Point 253 °C
487 °F
B/120; ISO 306
Sax Polymers SAXAMID 226F6RY01 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6RY01 is a polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Vicat Softening Point 253 °C
487 °F
B/120; ISO 306
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded
AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
Vicat Softening Point 253 °C
487 °F
A/50; ISO 306
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded
Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar.
Vicat Softening Point 253 °C
487 °F
B/120; ISO 306
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded
AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Copyright © lookpolymers.com All Rights Reserved