Polymer Property : Vicat Softening Point = 239 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 130 - 239 °C
266 - 462 °F
Average value: 156 °C Grade Count:9
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Vicat Softening Point 146 - 239 °C
295 - 462 °F
Average value: 196 °C Grade Count:9
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..