Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 206 °C | 403 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Vicat Softening Point | 206 °C | 403 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Vicat Softening Point | 206 °C | 403 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP THERMOCOMP PF004 PA 6 (Europe-Africa-Middle East) 20% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Vicat Softening Point | 206 °C | 403 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 206 °C | 403 °F | B/120; ISO 306 |
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 206 °C | 403 °F | B/120; ISO 306 |
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 206 °C | 403 °F | 10 N - A method; ISO 306 |
Arkema Group Orgalloy® LE 60 SF Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Vicat Softening Point | 206 °C | 403 °F | B/120; ISO 306 |
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 206 °C | 403 °F | B/120; ISO 306 |
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 206 °C | 403 °F | 50 N; 120 °C/h; ISO 306 |
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |