Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 90.7 °C | 195 °F | 0.125 inch bar, 1 Kg; ASTM D1525 |
Network Polymers SBS 1000 Clear Styrene Butadiene Copolymer Description: Clear Styrene Butadiene CopolymerInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 90.7 °C | 195 °F | ASTM D1525 |
Network Polymers Softflex® 1104 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 90.6 °C | 195 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
Vicat Softening Point | 90.6 °C | 195 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Vicat Softening Point | 90.6 °C | 195 °F | 120°C/hr, 9.8N; ASTM D1525 |
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Vicat Softening Point | 90.7 °C @Load 1.00 kg, Thickness 3.17 mm |
195 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers SBS 1031 Clear Styrene Butadiene Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 90.3 °C | 195 °F | |
Dow Primacor® 1321 Ethylene Acrylic Acid (EAA) PRIMACOR® 1321 polymer is an EAA copolymer (% comonomer 6.5) for blown and cast films. Its outstanding properties include, excellent sealability, toughness, adhesion and tear resistance. PRIMACOR 1.. |